Wrought Superalloy GH3030 alloy
Wrought Superalloy GH3030 alloy 1.80Ni-20Cr Solid-solution strengthened high temperature alloy has simple chemical composition. It has good anti-oxidation, heat resistant, cold pressing and welding capability. It can work under 800℃ normally with stable organization. It becomes single-phrase austenitic after solid-solution and can bear large stress for long time under high temperature. GB: GH3030(GH30) TOCT: XH78T Chemical component
C Si Mn P S Cr Ni Al Ti Fe ≤0.12 ≤ 0.80 ≤ 0.70 ≤ 0.030 ≤ 0.020 19.00- 22.00 balance ≤ 0.15 0.15- 0.35 ≤ 1.50
4.Mechanical property
yield strength ó 0.2/MPa |
tensile strength ó b/MPa |
Elongation δ5% |
320 |
635 |
35 |
5.Physics capability
density:8.4g/cm3 melting point:1374-1420℃
6.Application
Mainly used in the firebox part under 800℃ of turbine engine and other high temperature parts under
1100℃ with.
Making the high temperature parts of aviation and spaceflight engine.
The high temperature material of industrial wheel, energy, chemical and so on.
Please feel free to contact me at my email vivian (at) baoyuansteel (dot) com if you need above material.
Best regards
Vivian Zheng
Sales
Shanghai Baoyuan Metal Materials Co.,Ltd
Add: No .188 ,Xinchun Road, Shanghai, China 201109
Tel: 0086 021 54192998-612
Fax: 0086 021 54192997
Website:
vivian(at)baoyuansteel(dot)com
Skype:vivianzheng1314